Product Properties:
PE Color Coated Aluminum Coil:
Xinyu PE color coated aluminum coil with good PE Paints and high performance of aluminum coil is produced by advanced roller coating. All performance parameters are up to or much higher than related national standards.
Characteristic:
1) High gloss
2) Multi-choice colors
3) Impact resistance
4) Easy for processing
Performance:
The performance of PE color coated coil
1)Thickness≤0.5mm
Item | Test Item | Standard | National standard | Test Result |
1 | Color Difference | ECCA T3 | ΔE≤2.0 | ΔE≤1.5 |
2 | Gloss Difference | ECCA T2 | ≤10 | ≤5 |
3 | Coating Thickness | ECCA T1 | Min 14µm | ≥16µm |
4 | Pencil Hardness | ASTM D3363 | ≥HB | HB |
5 | T-bend | ASTM D4145 | ≤3T | ≤2T |
6 | Adhesion | ASTM D3359 | Grade 0 | Grade 0 |
7 | Impact | ASTM D2794 | ≥20kg.cm | ≥20kg.cm |
8 | Boiling water Resistance | GB/T17748 | 2h no change | 2h no change |
9 | Solvent Resistance | ASTM D2248 | 200 times paint remaining | 200 times paint remaining |
10 | Salt Resistance | ASTM B117 | 720 hrs≤grade 1 | 720hrs≤grade 1 |
11 | Dirt Resistance | GB/T9780 | ≤5% | <5% |
12 | Color retaining | GB/T16259 | 600hrs △E≤2.0 | △E≤2.0 |
13 | Gloss weaken Level | 600hrs ≤ grade 2 | 600hrs ≤ grade 2 | |
14 | Chalking | 600hrs No Change | No Change |
2)Thickness>0.5mm
Item | Test Item | Standard | National standard | Test Result |
1 | Color Difference | ECCA T3 | ΔE≤2.0 | ΔE≤1.5 |
2 | Gloss Difference | ECCA T2 | ≤10 | ≤5 |
3 | Coating Thickness | ECCA T1 | Min 14µm | ≥18µm |
4 | Pencil Hardness | ASTM D3363 | ≥HB | HB |
5 | T-bend | ASTM D4145 | ≤3T | ≤2T |
6 | Adhesion | ASTM D3359 | Grade 0 | Grade 0 |
7 | Impact | ASTM D2794 | ≥50kg.cm | ≥50kg.cm |
8 | Boil Resistance | GB/T17748 | 2hrs No change | 2hrs No change |
9 | Solvent Resistance | ASTM D2248 | 200 times paint remaining | 200 times paint remaining |
10 | Salt Resistance | ASTM B117 | 720hrs ≤ grade 1 | 720hrs ≤ grade 1 |
11 | Acidity Resistance | GB/T9780 | ≤5% | <5% |
12 | Color retention | GB/T16259 | 600hrs △E≤2.0 | △E≤2.0 |
13 | Gloss weaken Level | 600hrs ≤grade 2 | 600hrs ≤ grade 2 | |
14 | Chalking | No change | No change |
Certification:
Packing:
Plate/coil is placed to the iron or wooden pallet ,wrapped by water-proof craft paper perfectly , then fixed by iron narrow belt well .
1)Packaging Detail:Package
2)Port:Qingdao port or other main port in China
3)Container:20ft GP:5898mm(Length)x2352mm(Width)x2393mm(High) , loading 18~25 tons .
40ft GP:12032mm(Length)x2352mm(Width)x2393mm(High) , loading 20~28 tons.